Crystal-plasticity-finite-element modeling of the quasi-static and dynamic response of a directionally solidified nickel-base superalloy


Journal article


R. Sancho, J. Segurado, B. Erice, M.-J. Pérez-Martín, F. Gálvez
Materials, vol. 13, 2020, pp. 1-15

Cite

Cite

APA   Click to copy
Sancho, R., Segurado, J., Erice, B., Pérez-Martín, M.-J., & Gálvez, F. (2020). Crystal-plasticity-finite-element modeling of the quasi-static and dynamic response of a directionally solidified nickel-base superalloy. Materials, 13, 1–15.


Chicago/Turabian   Click to copy
Sancho, R., J. Segurado, B. Erice, M.-J. Pérez-Martín, and F. Gálvez. “Crystal-Plasticity-Finite-Element Modeling of the Quasi-Static and Dynamic Response of a Directionally Solidified Nickel-Base Superalloy.” Materials 13 (2020): 1–15.


MLA   Click to copy
Sancho, R., et al. “Crystal-Plasticity-Finite-Element Modeling of the Quasi-Static and Dynamic Response of a Directionally Solidified Nickel-Base Superalloy.” Materials, vol. 13, 2020, pp. 1–15.


BibTeX   Click to copy

@article{sancho2020a,
  title = {Crystal-plasticity-finite-element modeling of the quasi-static and dynamic response of a directionally solidified nickel-base superalloy},
  year = {2020},
  journal = {Materials},
  pages = {1-15},
  volume = {13},
  author = {Sancho, R. and Segurado, J. and Erice, B. and Pérez-Martín, M.-J. and Gálvez, F.}
}


Share

Text Only Owlstown
QR Code
Translate to