An experimental and numerical study of ductile failure under quasi-static and impact loadings of Inconel 718 nickel-base superalloy


Journal article


B. Erice, M.J. Pérez-Martín, F. Gálvez
International Journal of Impact Engineering, vol. 69, 2014, pp. 11-24

Cite

Cite

APA   Click to copy
Erice, B., Pérez-Martín, M. J., & Gálvez, F. (2014). An experimental and numerical study of ductile failure under quasi-static and impact loadings of Inconel 718 nickel-base superalloy. International Journal of Impact Engineering, 69, 11–24.


Chicago/Turabian   Click to copy
Erice, B., M.J. Pérez-Martín, and F. Gálvez. “An Experimental and Numerical Study of Ductile Failure under Quasi-Static and Impact Loadings of Inconel 718 Nickel-Base Superalloy.” International Journal of Impact Engineering 69 (2014): 11–24.


MLA   Click to copy
Erice, B., et al. “An Experimental and Numerical Study of Ductile Failure under Quasi-Static and Impact Loadings of Inconel 718 Nickel-Base Superalloy.” International Journal of Impact Engineering, vol. 69, 2014, pp. 11–24.


BibTeX   Click to copy

@article{erice2014a,
  title = {An experimental and numerical study of ductile failure under quasi-static and impact loadings of Inconel 718 nickel-base superalloy},
  year = {2014},
  journal = {International Journal of Impact Engineering},
  pages = {11-24},
  volume = {69},
  author = {Erice, B. and Pérez-Martín, M.J. and Gálvez, F.}
}


Share

Text Only Owlstown
QR Code
Translate to